On 6 and 7 station part formers — stronger parts, less scrap, high volumes for automotive & industry.
Cold forging is what we do first and what we do most. If you buy fasteners or small steel components in volume, it's very likely the most economical way to make them.
Wire coil is cut to blank, then formed at room temperature across multi-station dies — upset, extrude, pierce. Metal grain flows with shape, not cut away.
Where you need strength + volume + cost control — that's where cold forging wins.
Deep undercuts / odd cross-holes need secondary machining. Cost adds.
50-100 pcs — machining from bar is cheaper. Forging pays at volume.
Our sweet spot M3-M16 type. Beyond that — hot forging route better.
Take a length of steel wire. Cut a short slug from it. Now press that slug into a hardened die with enough force that the steel flows like stiff clay and takes shape of the cavity.
Do it again in next die, and next. A few hits later you have a part.
No heating. No chips. That's cold forging. "Heading" is older name — from days when main job was to form head on a bolt.
Wire → SlugLength cut from coil, grade per drawing
Press in DieSteel flows like clay into cavity
Next Die, NextEach station adds shape
Finished PartA few hits = near net shape
Our part formers do this at high speed across six or seven stations in a row, moving each blank from die to die with transfer fingers.
No heating. No chips. That's why it's cheaper, stronger, less scrap vs bar machining.
Not marketing — 4 real reasons. Grain, hardening, material, speed.
When steel is cut on a lathe, tool slices through its grain. When steel is forged, grain bends and follows shape. Loads travel along those lines instead of across them, so part resists fatigue and shock better.
Squeezing steel cold makes it harder and stronger than it was as wire. For some parts that's enough to meet strength requirement without heat treatment.
Machining a hollow bush from bar can turn more than half the steel into swarf. Forging same bush uses almost everything that goes in.
A part former turns out parts many times faster than a lathe, and every one comes from same die, so they're alike.
Not marketing — 4 real reasons. Grain, hardening, material, speed.
When steel is cut on a lathe, tool slices through its grain. When steel is forged, grain bends and follows shape. Loads travel along those lines instead of across them, so part resists fatigue and shock better.
Squeezing steel cold makes it harder and stronger than it was as wire. For some parts that's enough to meet strength requirement without heat treatment.
Machining a hollow bush from bar can turn more than half the steel into swarf. Forging same bush uses almost everything that goes in.
A part former turns out parts many times faster than a lathe, and every one comes from same die, so they're alike.
With multi-station formers, a lot of geometry can be produced straight off the machine.
Hexagon, round, square and flanged heads
Stepped diameters and shoulders
Flanges and collars
Blind and through holes
Hollow and tubular sections
Knurls, serrations and weld projections
Spherical ball forms
Internal recesses and counterbores
Having this spread lets us run each part on a machine suited to its size. A small T-weld nut doesn't belong on largest former, and wheel nut won't fit on smallest.
Right machine = right cost. We don't force small part on big former — saves tooling, saves time, saves your price.
Cold forging needs steel that can flow without cracking. The usual choices are low and medium carbon cold heading grades, boron steels for parts that will be hardened, and alloy steels for high strength classes.
The grade is always fixed by your drawing or agreed with you beforehand.
We don't change grade without approval. Your drawing decides — or we agree together before tooling.
Forging needs dedicated tooling, so it pays back on volume. For few hundred pieces a year, machining is wiser — and we'll say so.
Cold forging can't do everything. Very sharp internal corners, deep narrow grooves, cross holes and extremely tight bore tolerances normally need secondary operation.
We plan those in from start. Punching, tapping, thread rolling and machining are all part of our route, so part still leaves us finished.
Study drawing / sample — size, grade, tolerances, volume
Forging sequence — station by station design
Tooling designed & made — dies, punches in-house
Trials & measurement — samples measured on all criticals
Samples to you — for approval
Regular production — once you're satisfied
For most features, yes. Critical dimensions that need more are finished by machining.
Cold forging suits repeat production. Share annual volume and we'll tell you whether tooling is justified.
Often we can, and sometimes with small design tweak that makes it forge better. We'll suggest it; decision is yours.
Only if strength grade requires it.
If component is costing too much in material or machining time, cold forging might be answer. Email drawing to info@fastenertech.in